EP51FL
Two component room temperature curing epoxy system for bonding, sealing and coating
Key Features
- Good toughness and flexibility
- Easy handling
- Very rapid curing
- Cryogenically serviceable
Typical Properties
Viscosity
Part A: 3,000-10,000 cps, Part B: 50,000-90,000 cps
Cure Schedule
75°F: 12-24 hours; 150-200°F: 1 hour
Hardness
75-80 Shore D
Service Temperature Range
4K to +250°F
Dielectric Constant
3.3
Volume Resistivity
>10¹⁵ ohm-cm