EP21FL
Toughened, two component epoxy for bonding, sealing and encapsulation
Key Features
- Withstands rigorous thermal cycling
- Superior durability
- Low exotherm during cure
- Long working life
- Cures at ambient temperatures
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
2,000-4,500 cps
Cure Schedule
Optimum cure schedule: overnight at 75°F plus 2-3 hours at 150-200°F
Hardness
40-50 Shore D
Service Temperature Range
-100°F to +250°F
Tensile Modulus
150,000-200,000 psi
Volume Resistivity
10¹⁴ ohm-cm