EP21TDC-7

Two component, highly flexibilized epoxy for bonding, sealing and coating
Key Features
  • High peel strength
  • Outstanding adhesion to rubbers
  • Excellent thermal cycling resistance
  • Good electrical insulator
Typical Properties
Viscosity
Part A: 9,000-14,000 cps, Part B: 200,000-300,000 cps
Cure Schedule
12 hours at 75°F followed by 3-5 hours at 140-160°F
Hardness
65-75 Shore A
Service Temperature Range
-100°F to +250°F
Elongation
>200%
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
EP21TDC-7 Two Component Epoxy
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP21TDC-7 is a two component, very flexible epoxy system for high performance bonding, sealing and coating. It has a non-critical one to seven mix ratio by weight. EP21TDC-7 has a room temperature cure that can be accelerated by adding heat. The optimum cure schedule is 12 hours at 75°F followed by 3-5 hours at 140-160°F. An unusual feature of this product is that straight heat curing results in a product that is slightly softer (40-50 Shore A), than the one with the optimum cure (65-75 Shore A). The cured system has a peel strength greater than 25-35 pli and an elongation of over 200%. EP21TDC-7 bonds well to a wide variety of metals, plastics and especially rubbers. In fact, it usually adheres well to rubbers such as neoprene, nitrile, SBR and occasionally EPDM, although surface treatment of the rubbers (especially EPDM) will allow for better adhesion. The cured system has excellent electrical insulation properties along with good chemical resistance to oils and water. The epoxy has superior resistance to rigorous thermal cycling along with an outstanding ability to resist mechanical shock and vibration. EP21TDC-7 has a relatively long open time of 90-120 minutes for a 100 gram mass. The color of Part A is clear and Part B is amber-brown. It has an operating temperature range of -100°F to +250°F. It can be used in aerospace, electrical, OEM, electronic as well as repair and maintenance applications, where the special properties described above are desirable.

Product Advantages

  • Non-critical, one to seven mix ratio, by weight, available in pre-measured kits
  • High peel strength
  • Withstands rigorous thermal cycling and shock
  • Bonds especially well to rubber including neoprene, nitrile, SBR and occasionally EPDM
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.