EP21TDCHT-LO

Versatile, toughened two component epoxy for bonding, sealing and coating
Key Features
  • Superb strength profile
  • Withstands aggressive thermal cycling
  • Dependable electrical insulator
  • Meets NASA specifications for low outgassing
  • Ideal for bonding similar and dissimilar substrates
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 60,000-110,000 cps, Part B: 70,000-140,000 cps
Cure Schedule
overnight at 75°F, followed by 2-3 hours at 200°F, although a straight heat cure at 150-200°F for 2-3 hours is also acceptable
Hardness
65-75 Shore D
Service Temperature Range
-100°F to +350°F
Tensile Lap Shear Strength
2,600-2,800 psi
Tensile Modulus
200,000-250,000 psi
תמונה
EP21TDCHT-LO Two Component Epoxy Adhesive
Certifications

1,000 Hours at 85°C/85% RH

ASTM E595 Compliant

Meets EU Directive 2015/863

Product Description

Master Bond EP21TDCHT-LO is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving one to one mix ratio by weight. The recommended cure schedule being overnight at room temperature, followed by 2-3 hours at 200°F, although a straight heat cure at 150-200°F for 2-3 hours is also acceptable. This moderate viscosity system bonds well and with minimum shrinkage to a wide variety of substrates including metals, composites, glass, ceramics and many plastics and rubbers. EP21TDCHT-LO combines good dimensional stability with toughness. The forgiving nature of EP21TDCHT-LO allows it to be used for bonding dissimilar substrates that might have different coefficients of thermal expansion, conferring upon it top notch resistance to rigorous thermal cycling as well as vibration and shock. Additionally, it is a superior electrical insulator and has good chemical resistance against water, fuels and oils. Its service temperature range is from -100°F to +350°F. Part A is clear and Part B is amber in color. It can be used in aerospace, electronic, vacuum, semiconductor and specialty OEM applications where low outgassing and the properties mentioned previously are desirable.

Product Advantages

  • Convenient mixing: forgiving one to one ratio by weight
  • User friendly, easy to apply, good flow along with convenient curing schedules
  • Impressive adhesion to a wide variety of substrates
  • Very good toughness, can withstand harsh thermal cycling while retaining dimensional stability
  • Dependable electrical insulation values
  • Passes NASA low outgassing requirements
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.