EP21TPFL-1AO

Flexible two component epoxy polysulfide system for high performance bonding, sealing, coating and potting
Key Features
  • Room temperature curing
  • Excellent thermal conductivity
  • Superior electrical insulation
  • Low viscosity and good flow properties
  • Withstands rigorous thermal cycling
  • Reliable resistance to fuels and oils
Typical Properties
Viscosity
Part A: 15,000-30,000 cps, Part B: 14,000-28,000 cps
Cure Schedule
75°F, 3-5 days
Hardness
70-90 Shore A
Service Temperature Range
-60°F to +250°F
Dielectric Constant
4.5
Elongation
150-200%
תמונה
EP21TPFL-1AO Two Part Epoxy Polysuifide System
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP21TPFL-1AO is a two component, low viscosity epoxy polysulfide for high performance bonding, sealing, coating and encapsulation. The main focus of this material is genuinely good thermal conductivity and electrical insulation properties, as well as a high degree of flexibility. This enables EP21TPFL-1AO to be used in situations with intense thermal cycling along with thermal and mechanical shock. Its lower viscosity and easy flow make it well suited for many potting and encapsulation applications. Additionally, being a polysulfide based system, it has very good chemical resistance, particularly to fuels, oils, hydraulics and related compounds.

The handling is relatively straightforward. The mix ratio is a forgiving two to three by weight or volume. Upon mixing, the open time is conveniently long. It has very good adhesion to metals, ceramics, composites, glass, and many rubbers and plastics. The system should not be heated and will crosslink fully 3-5 days. The service temperature range is -60°F to +250°F. The system is color coded for easy mixing, Part A is black while Part B is off-white. This unusual blend of properties; specifically, flexibility, thermal conductivity chemical resistance, allows EP21TPFL-1AO to be a prime candidate for specialty applications in the electronic, aerospace, specialty OEM and related industries.

Product Advantages

  • Easy to handle; forgiving mix ratio
  • Superb thermal conductivity and electrical insulation values
  • Exceptional flexibility, withstands aggressive thermal cycling
  • Stellar chemical resistance profile
  • Fully cures at ambient temperatures
  • Lower viscosity, well suited for potting and encapsulation
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.