UV10TKLO-2
One component UV-curable system for bonding, sealing and encapsulation
Key Features
- High viscosity system
- Meets NASA low outgassing specifications
- Very good temperature resistance profile
- Excellent optical clarity
- Withstands harsh chemicals
- Fast curing upon exposure to UV light source
Typical Properties
Viscosity
225,000-275,000 cps
Cure Schedule
UV light 320-365 nm for 20-30 seconds
Hardness
80-85 Shore D
Service Temperature Range
-60°F to +400°F
Dielectric Constant
3.6
Tensile Modulus
>200,000 psi
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863
Case Study
UV10TKLO-2: Used to adhere mirrors in a Kirkpatrick-Baez microscope to image X-ray emissions during deuterium-tritium implosions
UV10TKLO-2 is suitable for use in applications that involve the use of a vacuum, including optical equipment such as Kirkpatrick–Baez (KB)–type X-ray microscopes to measure the performance of a fuel used in nuclear fusion.1 Download the full case stu …