UV15

Low viscosity, one component, UV curable epoxy based system
Key Features
  • Low viscosity
  • Exceptional thermal stability
  • Cationic curing system
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
115-350 cps
Cure Schedule
Cures in thicknesses of a few microns to 0.015-0.020 inches in 15-30 seconds or less.
Hardness
>75 Shore D
Service Temperature Range
-80°F to +350°F.
Glass Transition Temperature (Tg)
90-95°C with a straight UV cure; 125-130°C when post cured for 30 minutes at 125°C.
Refractive Index
1.517
תמונה
UV15 One Part UV Curable Compound
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

IEC 61249-2-21 for Halogen Free

Product Description

Master Bond UV15 is a high strength, low viscosity, epoxy based UV curable system for bonding, sealing and coating. It is 100% reactive and does not contain any solvents or other volatiles. It is also completely free of any oxygen inhibition. UV15 will cure quickly and easily when exposed to a UV light source with a wavelength range between 320-365 nm, with the optimum at 365 nm. The energy required is typically 20-40 milliwatts per cm². The rate of cure depends upon the distance of the light from the material being cured, the thickness of the section and the intensity of the light source. It typically cures in thicknesses of a few microns to 0.015-0.020 inches in 15-30 seconds or less. Epoxy based UVs are described as having a cationic curing reaction. This kind of system will have lower shrinkage (1-2%) and higher temperature resistance than the majority of UV systems, which cure by a free radical mechanism. UV15 has excellent resistance to a wide variety of chemicals including water, acids, bases, fuels and many solvents. It features superb physical strength characteristics and electrical insulation properties. UV15 has superior adhesion to a wide variety of substrates including plastics, glass and many metals. As is typical with UVs, it has excellent optical clarity and light transmission properties. It is important to note that UV15’s low viscosity allows it to be spin coated.

Cationic systems, such as UV15, tend to have much higher temperature resistance than other UV type systems. Its glass transition temperature (Tg) with a straight UV cure is 90-95°C, and when post cured for 30 minutes at 125°C, the Tg is 125-130°C. This post cure also enhances UV15’s chemical resistance. The service temperature range for this system is -80°F to +350°F. It is widely used for a variety of applications in the optical, optoelectronic, aerospace and related industries.

Product Advantages

  • One component system; no mixing needed
  • Very low viscosity, easily applied; readily spin coated
  • Cationic curing, no oxygen inhibition
  • Superior temperature resistance, especially when post cured with heat
  • Outstanding optical clarity and light transmission
  • Good adhesion to many substrates
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.