UV15LV
Low viscosity, one component, UV curable epoxy based system
Key Features
- Exceptionally low viscosity
- Superior thermal stability
- Very little shrinkage upon cure
- Cationic curing system
Typical Properties
Viscosity
70-120 cps
Cure Schedule
UV light 320-365 nm for 15-30 seconds
Hardness
>75 Shore D
Service Temperature Range
-80°F to +300°F
Dielectric Constant
3.25
Refractive Index
1.517
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Certifications
Meets EU Directive 2015/863
Case Study
UV15LV Citation
Master Bond UV15LV was used in a research article for photo-stability measurements of electropoptic polymer inverted ridge waveguides. For this application, UV curable epoxy Master Bond UV15LV1 was used to spin coat silicon wafers, to form claddings. …