EP21LV-LO

Two component, low viscosity NASA low outgassing epoxy compound
Key Features
  • One to one mix ratio by weight
  • High bond strength
  • Superior electrical insulation properties
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
10,000-13,000 cps
Cure Schedule
overnight at 75°F followed by 2 hours at 150-200°F
Hardness
70-80 Shore D
Service Temperature Range
-65°F to +250°F
Dielectric Constant
2.79
Tensile Lap Shear Strength
2,600-2,800 psi
תמונה
EP21LV-LO Two Part Epoxy
Certifications

1,000 Hours at 85°C/85% RH

Meets EU Directive 2015/863

ASTM E595 Compliant

Product Description

Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user friendly system has an easy and convenient one to one mix ratio by weight. EP21LV-LO features outstanding physical strength properties, along with being an excellent electrical insulator. This combination of properties enables it to be readily used as a potting and encapsulation compound. EP21LV-LO resists many chemicals including water, oils, fuels, acids, bases and salts quite well. It bonds well to a variety of substrates including metals, glass, ceramics and many types of rubber and many plastics. Although the EP21LV-LO can cure at room temperature, to optimize its properties, it is recommended that the system cures for 12-24 hours at room temperature, plus another 2 hours at 150-200°F. Most importantly, EP21LV-LO passes NASA low outgassing specifications. The color of Part A is clear and Part B is amber-clear in color. It is serviceable over the wide temperature range of -60°F to +250°F. This exceptionally versatile system can used in aerospace, microelectronics, semiconductor, optical and vacuum applications.

Product Advantages

  • Lower viscosity; convenient handling
  • Easily applied; adhesive spreads smoothly
  • High bonding strength to a wide variety of substrates
  • Good electrical insulation properties
  • Superior durability, thermal shock and chemical resistance
  • Passes NASA low outgassing specifications
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.