Thermally Conductive, Electrically Insulative One Part Epoxy for Die Attach Applications
Formulated for die attach applications, Master Bond Supreme 3HTND-2DA is a fast curing, high performance one component epoxy system. It cures in 5-10 minutes at 150°C and has unlimited working life at room temperature. It is available in syringes and has a shelf life of 6 months when stored at 40-50°F.
Supreme 3HTND-2DA has a die shear strength of 19-21 kg-f and performed very well in 85/85 testing. This epoxy has excellent adhesion to metals, ceramics and silicon dies. It is serviceable over the wide temperature range of -100°F to +400°F. As a toughened system, it offers the ability to withstand rigorous thermal cycling and shock.
In accordance with die attach application requirements, this product passes NASA low outgassing test specifications. Supreme 3HTND-2DA has low ionics, particularly chlorine (<15 ppm). It also features dimensional stability, superior thermal conductivity, electrical insulation properties and a glass transition temperature of 100-105°C.
Unlike many other die attach systems, Supreme 3HTND-2DA is not premixed and frozen, but it requires refrigeration for storage. This system dispenses smoothly or without any tailing. It well suited for automatic dispensing equipment. With a viscosity of over 300,000 cps (thixotropic), it can be applied to a defined area without running.
For Editorial Use
Click below to download this release in the format of your choice.
| צְרוּפָה | גודל |
|---|---|
| Supreme 3HTND-2DA_nr.doc (28.69 KB) | 28.69 KB |
| צְרוּפָה | גודל |
|---|---|
| Supreme 3HTND-2DA_nr.html (28.69 KB) | 28.69 KB |
| צְרוּפָה | גודל |
|---|---|
| Supreme 3HTND-2DA_nr.txt (345 bytes) | 345 bytes |
News Release Images
Click an image to download a high resolution version in JPEG format.