EP45HTAN

Two component, high strength epoxy system
Key Features
  • Easy to work with
  • Thermally conductive and electrically insulative
  • Superior dimensional stability
  • Excellent strength retention at high temperatures
  • Cryogenically serviceable
  • Bonds well to metals, especially roughened titanium
Typical Properties
Viscosity
thixotropic paste
Cure Schedule
2-3 hours at 300°F followed by a post cure of 3-4 hours at 350°F
Hardness
80-90 Shore D
Service Temperature Range
4K to +500°F
Dielectric Constant
4.6
Tensile Lap Shear Strength
2,300-2,500 psi
תמונה
EP45HTAN Two Part Epoxy
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP45HTAN is a two component, thermally conductive, electrically insulative epoxy for bonding and sealing. The mix ratio is a forgiving 100 to 30 by weight. Parts A and B are thixotropic pastes. lt is 100% reactive and does not contain any solvents or diluents. EP45HTAN does not cure at ambient temperatures and requires an elevated temperature cure. The optimum cure is 2-3 hours at 300°F followed by a post cure of 3-4 hours at 350°F. Although it is a thixotropic paste, it will flow slightly when being cured.

This epoxy combines cryogenic temperature serviceability along with high temperature resistance. It bonds well to a wide variety of substrates, such as metals, glass, composites and many plastics. Its service temperature range is 4K to +500°F. It withstands tough chemical environments ranging from exposure to water, oils and fuels, as well as many acids and bases. The color of Parts A and B is gray. Some other desirable features of this system include its dimensional stability and low shrinkage upon cure. EP45HTAN can be used in the aerospace, electronic, specialty OEM, oil and gas processing, among other industries where extreme low and high temperature resistance and thermal conductivity are important requirements.

Product Advantages

  • Forgiving mix ratio
  • Easily applied, paste-like viscosity
  • Exceptionally long pot life at room temperature
  • Cryogenically serviceable as well as high temperature resistant
  • Superior adhesive properties
  • Thermally conductive and electrically insulating
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.