Thermally Conductive, High Temperature Resistant Epoxy Passes NASA Low Outgassing Tests
Certified to meet ASTM E595 NASA low outgassing standards, Master Bond EP46HT-2AO Black is well suited for the aerospace, electronic, opto-electronic industries and can be used vacuum environments. This two component system blends thermal stability with a high strength profile for a variety of bonding, sealing and encapsulation applications.
EP46HT-2AO Black combines superior thermal conductivity of 9-10 BTU•in/ft2•hr•°F [1.2981-1.4423 W/(m·K)] and reliable electrical insulation with a volume resistivity exceeding 1014 ohm-cm at room temperature. It has a glass transition temperature of 200-210°C and is serviceable over the wide temperature range of -100°F to +500°F [-73°C to +260°C]. This dimensionally stable system delivers a tensile strength of 6,000-7,000 psi, compressive strength of 26,000-28,000 psi and tensile lap shear strength of 1,400-1,600 psi at 75°F. EP46HT-2AO Black also withstands a variety of chemicals including oils, water, acids, bases and fuels.
Unlike most traditional two part epoxies, EP46HT-2AO Black cures with the addition of heat, which allows it to have a working life of over 24 hours. It has a forgiving 100 to 30-35 mix ratio by weight and upon mixing, this thixotropic system has a viscosity of 140,000-280,000 cps. It bonds well to metals, composites, glass, ceramics, rubbers and many plastics.
This epoxy is available in ½ pint, pint, quart, gallon and 5 gallon container kits. Part A of this system is black in color and Part B is gray. EP46HT-2AO Black has a minimum 6 month, maximum 1 year shelf life at ambient temperatures in original, unopened containers.
For Editorial Use
Click below to download this release in the format of your choice.
| צְרוּפָה | גודל |
|---|---|
| EP46HT-2AO Black_nr.doc (28.68 KB) | 28.68 KB |
| צְרוּפָה | גודל |
|---|---|
| EP3HTND-2Med_Black_nr.html (3.68 KB) | 3.68 KB |
| צְרוּפָה | גודל |
|---|---|
| EP3HTND-2Med_Black_nr.txt (2.88 KB) | 2.88 KB |
News Release Images
Click an image to download a high resolution version in JPEG format.