- Low coefficient of thermal expansion
Typical Properties
Viscosity
40,000-80,000 cps
Cure Schedule
Cure in 3-4 days at 75°F or 2-3 hours at 150-200°F; Recommended curing is overnight at 75°F followed by 2-3 hours at 150-200°F; Optimum cure schedule: Overnight at 75°F, followed by 2-3 hours at 150-200°F
Hardness
85-95 Shore D
Service Temperature Range
4K to +400°F
Acoustical Impedance
5.3 MRayl
Glass Transition Temperature (Tg)
140-150°C
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
ASTM E595 Compliant
Packaging
וידאו
How Do You Mix a Thick Part A with a Thin Part B of an Epoxy?
Watch this video to see the process of how to mix epoxy system EP42HT-3AO with a thick Part A component and a thin Part B component.Learn how to properly weigh and mix the material to reach the desired consistency.