MasterSil 151TC

Two part, room temperature curing, thermally conductive silicone with ultra fine particle filler for bonding and smaller gap filling
Key Features
  • High thermal conductivity
  • Very good electrical insulator
  • High flexibility and temperature resistance
  • Meets NASA low outgassing specifications
Typical Properties
Viscosity
30,000-60,000 cps
Cure Schedule
Optimum cure is overnight at 75°F followed by 1-2 hours at 150-200°F.
Hardness
80-90 Shore A
Service Temperature Range
-65°F to +400°F
Dielectric Strength
450 volts/mil
Thermal Conductivity
4.0-5.8 BTU•in/(ft²•hr•°F)
תמונה
MasterSil 151TC Two Part Silicone
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond MasterSil 151TC is a two component silicone for use primarily in thermal management applications. It is primarily used for bonding or smaller gap filling. It has very fine particles of a thermally conductive filler that allows it to be applied in sections as thin as 10-15 microns. It has a 100 to 4 mix ratio by weight, and upon mixing, flows evenly and smoothly. It will cure in 2-3 hours at 150-200°F or in 2-3 days at room temperature. The optimum cure is overnight at room temperature followed by 1-2 hours at 150-200°F.

MasterSil 151TC is an addition cured silicone offering both flexibility and high temperature resistance. Its inherent flexibility allows it to withstand severe thermal cycling as well as vibration and shock. Regarding its thermal transfer capabilities, the system combines high conductivity with very fine particle filler. This allow it to be applied in a very thin layer and lowers its thermal resistance to 7-10 x 10-6 K•m2/W. This is much better than more standard thermally conductive silicones. The service temperature range is -65°F to +400°F. The color of Part A is white and Part B is clear. MasterSil 151TC fits well in applications involving sensitive optical and electronic components where optimum heat dissipation is critical. The other main attributes are its flexibility and its ability to withstand high temperatures, as noted previously.

Product Advantages

  • Addition cured; no by-products released during cure; does not require air for curing
  • Low exotherm
  • Good flow properties
  • Can be applied in very thin sections
  • Very low shrinkage upon cure
  • Combines high thermal conductivity and low thermal resistance
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.