EP21TPND-NV

Two component, paste-like epoxy polysulfide for bonding, sealing and coating
Key Features
  • One to one mix ratio
  • Superior resistance to fuels and oils
  • Thixotropic paste
  • Room temperature curing compound
  • Withstands 1,000 hours 85°C/85% RH
  • Fully complies with RoHS regulations


Note: EP21TPND-NV complies with RoHS3 Directive (EU) 2015/863. It is a new version of EP21TPND, which has been discontinued.

Typical Properties
Viscosity
paste
Cure Schedule
48-72 hours at 75°F
Hardness
40-50 Shore D
Service Temperature Range
-80°F to +250°F
Dielectric Constant
3.7
Elongation
20-30%
תמונה
EP21TPND-NV Two Component Epoxy Polysulfide
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Packaging
Product Description

Master Bond EP21TPND-NV is a two component epoxy polysulfide system with a paste consistency that cures at room temperature or more rapidly at elevated temperatures. It has a forgiving one to one mix ratio by weight or volume and can be used as an adhesive, coating and sealant. It’s very resistant to a number of chemicals including water, gasoline, fuels, oils, hydrocarbons, hydraulic fluids and many acids and bases. Significantly, unlike many chemical resistant epoxy based materials, this system has excellent toughness and flexibility. The combination of properties enables EP21TPND-NV to withstand rigorous thermal cycling as well as mechanical and thermal shocks. It bonds well to a variety of substrates, including metals, glass, ceramics and many rubber and plastic materials. The cured system has excellent electrical insulation properties. Its service temperature range is -80°F to +250°F. One unusual feature of EP21TPND-NV is the influence of adding heat to the curing cycle. When cured at room temperature the Shore D hardness is 60-65 and when cured at 200°Ffor 2-3 hours, its hardness is 15-20 Shore D. Therefore, to optimize properties, especially its chemical resistance profile, room temperature curing only is recommended. The color of Part A is black and Part B is amber, although, other colors are available. Polysulfide based systems, including EP21TPND-NV, have been used as fuel tank sealants and as sealing compounds for electrical connectors exposed to fuels, oils and lubricants, for many years. EP21TPNDNV is also widely used in the aerospace, OEM, electronic, electrical, chemical and related industries.

Product Advantages

  • Easy mixing, forgiving 1:1 mix ratio, weight or volume
  • Smooth paste consistency, simple to apply
  • Ambient temperature curing imparts optimal chemical resistance and hardness
  • Forms tough bonds; resistant to thermal cycling
  • Bonds well to a variety of substrates
  • Superb resistance to oils, fuels and related chemicals
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.