EP30DP-NV

Toughened, two component epoxy for bonding, sealing, coating and encapsulation
Key Features
  • Low viscosity
  • Long working life
  • Cryogenically serviceable
  • RoHS compliant


Note: EP30DP-NV complies with RoHS3 Directive (EU) 2015/863. It is a new version of EP30DP, which has been discontinued.

Typical Properties
Viscosity
Part A: 5,000-8,000 cps, Part B: 250-500 cps
Cure Schedule
Optimal curing is overnight at 75°F followed by 2-4 hours at 150°F.
Hardness
30-50 Shore D
Service Temperature Range
4K to +250°F
Elongation
30-60%
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
EP30DP Two Part Epoxy
Product Description

Master Bond EP30DP-NV is a versatile, two component, epoxy system featuring superior toughness and abrasion resistance for high performance bonding, sealing, coating and encapsulation. It has an interesting chemistry where the rigidity of the epoxy is modified by the addition of a urethane based flexibilizer. This modification confers a lower Shore D hardness to the cross linked entity. It also enables a higher elongation than normally seen with basic epoxy compounds. It has a long working life, and after mixing, a low exotherm. It cures readily at ambient temperatures or more rapidly at elevated temperatures. Optimal curing is overnight at room temperature followed by 2-4 hours at 150°F. The system is 100% reactive and does not contain any solvents or diluents.

EP30DP-NV bonds well to a wide variety of substrates including metals, ceramics, composites, glass and many plastics. Its toughness allows it to withstand rigorous thermal cycling and shock as well as mechanically induced vibration. Also the epoxy-urethane backbone of this system gives it a higher level of abrasion resistance than more standard epoxy. It is also an excellent electrical insulator. This, combined with its low viscosity and low exotherm, allows it to be used for moderate to larger sized encapsulations. Another very special property is cryogenic serviceability with a temperature range extending from 4K to +250°F. The color of Part A is clear, and Part B is amber clear. EP30DP-NV can be used in electronics, aerospace, optical, specialty OEM and other applications where this product profile is desirable.

Product Advantages

  • Versatile curing options
  • Long working life and low exotherm
  • Toughened system
  • Excellent abrasion resistance
  • RoHS compliant
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.