EP37-3FLFAOND
Two component epoxy compound for bonding, sealing and encapsulation
Key Features
- Convenient handling
- High flexibility
- Paste consistency
- Thermally conductive and electrically insulative
- NASA low outgassing approved
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: paste, Part B: paste
Cure Schedule
75°F: 2-3 days; 150-200°F: 2-4 hours
Hardness
35-45 Shore D
Service Temperature Range
4K to +250°F
Dielectric Constant
4.9
Tensile Modulus
30,000-40,000 psi