Release Date: 09/17/2019
Product: Supreme 112
תמונה

High Tg, Ultra Low Viscosity Epoxy meets NASA Low Outgassing Specifications

Master Bond Supreme 112 is a new two part epoxy for bonding, sealing, potting, and impregnation applications. It is a heat curable system with a very low viscosity of 50-200 cps and a long open time of 2-3 days at room temperature for a 100 gram batch. Supreme 112 features a high glass transition temperature of 190-195°C and is serviceable up to 288°C (550°F). This compound bonds well to a variety of substrates including metals, composites, glass and ceramics. As a toughened system it withstands thermal cycling and mechanical stresses.

“Supreme 112 can be applied successfully not only in bonding applications, but it can also be used in porosity sealing. Additionally, it offers a high tensile strength of 11,000-12,000 psi”, says Rohit Ramnath, Senior Product Engineer. “This non-solvent based compound also meets NASA low outgassing requirements.”

Supreme 112 retains its electrical insulation properties even at elevated temperatures. While this system has a relatively easy to use mix ratio, 100:70 by weight, it requires a three step oven curing process of 1-2 hours at 200°F, followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Despite the long cure schedule, Supreme 112 offers a unique combination of performance properties advantageous in many applications in aerospace, electronic and automotive industries.

For Editorial Use

Click below to download this release in the format of your choice.

מסמך
צְרוּפָה גודל
Supreme-112_nr.doc (28.5 KB) 28.5 KB
מסמך
צְרוּפָה גודל
Supreme-112_nr.txt (5.93 KB) 5.93 KB
מסמך
צְרוּפָה גודל
Supreme-112_nr.html (3.84 KB) 3.84 KB