EP29LPAOHT

Two component, thermally conductive, electrically insulative epoxy system
Key Features
  • Low exotherm
  • Excellent flow properties
  • Superior dimensional stability
  • Well suited for large potting applications
Typical Properties
Viscosity
10,000-30,000 cps
Cure Schedule
overnight at 75°F followed by 4-6 hours at 150°F to 170°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +350°F
Coefficient of Thermal Expansion
22-24 x 10⁻⁶ in/in/°C
Volume Resistivity
>10¹⁵ ohm-cm
תמונה
EP29LPAOHT Two Part Epoxy
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP29LPAOHT is a two component epoxy system featuring good thermal conductivity along with being electrically isolating. It has convenient handling with a forgiving 100 to 50 mix ratio by weight. It is a low to moderate viscosity system with excellent flow properties. It can be mixed in masses over a gallon because it generates an exceptionally low exotherm. Additionally, it has a very long open time. The recommended cure schedule is overnight at room temperature followed by 4-6 hours at 150°F to 170°F. Also noteworthy is its very low shrinkage upon curing and dimensional stability.

This epoxy bonds well to a wide variety of substrates including metals, glass, ceramics and many different plastics. EP29LPAOHT is a very good heat conductor while retaining reliable electrical insulation values. It is resistant to water, fuels and oils. It has an array of other desirable properties including a high modulus, outstanding compressive strength, and a low coefficient of thermal expansion. Both Parts A and B are off white in color. The service temperature range is -60°F to +350°F. EP29LPAOHT is ideally suited for specialty potting applications where large amounts (up to and greater than 1 gallon) of epoxy will be poured at one time.

Product Advantages

  • Low to moderate viscosity
  • Flows smoothly and readily
  • Long working life at ambient temperatures
  • Good thermal conductivity
  • Meets NASA low outgassing
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.