Release Date: 10/30/2019
Product: EP62-1AO
תמונה

Thermally Conductive, Chemically Resistant Epoxy Sealant

Master Bond EP62-1AO is a two part epoxy adhesive and sealant with an exceptionally long working life of 12-14 hours at ambient temperature for a 100 gram mass. This makes it beneficial when bonding and sealing large or intricate parts that may need ample time for mixing and applying. This material has a high strength profile with a tensile modulus of 600,000 to 650,000 psi and a tensile strength of 5,000 to 6,000 psi. The service temperature range is -60°F to +450°F and it offers a glass transition temperature of 120-125°C.

EP62-1AO is both electrically insulating and thermally conductive with a thermal conductivity value of 9-10 BTU•in/(ft2•hr•°F), or 1.30-1.44 W/(m•K). Its chemical resistance profile is robust, especially when compared to other thermally conductive epoxies. It can withstand a wide range of acids, bases and solvents. EP62-1AO has a low coefficient of thermal expansion of 18-21 x 10-6 in/in/°C.

The viscosity of the mixed compound is of a thixotropic paste consistency. There are several cure schedule options to choose from, all of which require a relatively low heat activation. Additional post curing for 2 to 4 hours at 200-300°F is recommended to obtain optimal performance properties. It is available in 30 cc syringe kits, 1/2 pint kits, pint kits, and quart kits. The color of Part A is off white and Part B is dark brown.

For Editorial Use

Click below to download this release in the format of your choice.

מסמך
צְרוּפָה גודל
EP62-1AO_nr.doc (28.5 KB) 28.5 KB
מסמך
צְרוּפָה גודל
EP62-1AO_nr.txt (5.84 KB) 5.84 KB
מסמך
צְרוּפָה גודל
EP62-1AO_nr.html (3.77 KB) 3.77 KB