EP21DP12
Two component urethane modified epoxy for bonding, sealing and potting
Key Features
- Excellent toughness
- Convenient processing
- Can withstand rigorous thermal cycling
- Available in several colors
Typical Properties
Viscosity
Part A: 4,000-8,000 cps, Part B: 11,000-15,000 cps
Cure Schedule
overnight at 75°F followed by 2 to 3 hours at 135-150°F
Hardness
40-50 Shore D
Service Temperature Range
-100°F to +250°F
Dielectric Constant
3.8
Dielectric Strength
450 volts/mil
Tensile Modulus
5,000-15,000 psi
Volume Resistivity
>10¹⁴ ohm-cm