Supreme 11LV
Toughened, two component epoxy for bonding, sealing and coating
Key Features
- Convenient handling
- Good shear and peel strength
- Withstands thermal cycling
- Low modulus
Typical Properties
Viscosity
Part A: 1,000-4,000 cps., Part B: 24,000-30,000 cps.
Cure Schedule
75°F: 24-48 hours; 150°F: 1-2 hours.
Hardness
55-65. Shore D
Service Temperature Range
-100°F to +250°F
Coefficient of Thermal Expansion
55-60 X 10⁻⁶ in/in/°C.
Dielectric Constant
4.1.
T-peel Strength
15-25 pli.
Tensile Lap Shear Strength
1,500-1,700 psi.
Tensile Modulus
30,000-40,000 psi.
Volume Resistivity
>10¹³ ohm-cm.
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Certifications
Meets EU Directive 2015/863
Packaging