EP4S-80
One component, silver filled epoxy with a curing temperature of 80°C
Key Features
- Low viscosity
- Available in syringes and jars
- Good electrical conductivity
- NASA low outgassing
Typical Properties
Viscosity
10,000-15,000 cps
Cure Schedule
60-90 minutes at 80°C
Hardness
75-85 Shore D
Service Temperature Range
-76°F to +302°F
Glass Transition Temperature (Tg)
110-120°C
Volume Resistivity
<0.001 ohm-cm
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863
וידאו
One Part, Silver Filled Epoxy for EMI/RFI Shielding
Master Bond EP4S-80 is a one component, silver filled epoxy for bonding, sealing and coating. This NASA low outgassing approved system cures at the low temperature of 80˚C and bonds well to a variety of substrates. Watch this video to see how this lo …