EP51FL-1ND-2
Two component, fast curing epoxy for bonding, sealing and coating featuring high flexibility
Key Features
- Convenient handling
- Resists thermal cycling and shock
- Reliable electrical insulator
- Paste consistency
Typical Properties
Viscosity
Part A: 10,000-14,000 cps, Part B: 130,000-160,000 cps
Cure Schedule
30-40 minutes and full cure within 24 hours at 75°F; 2-3 hours at 75°F followed by an hour at 150-200°F
Hardness
10-20 Shore D
Service Temperature Range
-100°F to +250°F
Elongation
>200%
T-peel Strength
>30 pli
Volume Resistivity
>10¹⁵ ohm-cm