Supreme 42HT-2ND Black

Two component, non-flow epoxy system for bonding, sealing and coating
Key Features
  • Convenient processing
  • Superior thermal cycling capabilities
  • Meets NASA low outgassing specifications
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
paste
Cure Schedule
48-72 hours at ambient temperatures and in 2-3 hours at 200°F; optimum cure schedule is overnight at 75°F followed by 3-5 hours at 160-200°F
Hardness
75-85 Shore D
Service Temperature Range
4K to +450°F
Dielectric Constant
4.5
Glass Transition Temperature (Tg)
130-135 °C
תמונה
Supreme 42HT-2ND Black Two Part Epoxy
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Product Description

Master Bond Supreme 42HT-2ND Black is a special two part epoxy system combining robust temperature and chemical resistance, very good toughness and a smooth, non-flowing viscosity. Supreme 42HT-2ND Black is easy to use with a forgiving mix ratio of 100 to 40 by weight or 100 to 50 by volume. Supreme 42HT-2ND Black is a lower exotherm type system with a longer working life. It cures in 48-72 hours at ambient temperatures and in 2-3 hours at 200°F. The optimum cure schedule is overnight at room temperature followed by 3-5 hours at 160-200°F. The system is 100% reactive with no solvents or diluents, which imparts low shrinkage upon curing.

This epoxy bonds well to a wide variety of substrates including metals, composites, ceramics, glass and many plastics. Its toughness allows it to be well suited for bonding dissimilar substrates and to withstand rigorous thermal cycling. Additionally, the cured epoxy is a superb electrical insulator. It resists a wide range of chemicals including many acids, bases, solvents, fuels and oils. Its service temperature range is 4K to +450°F. The color of Part A is black and Part B is amber. This versatile system can be used in aerospace, electronic, optical and OEM industries, particularly when vacuum compatibility along with the other product properties mentioned previously are desirable.

Product Advantages

  • Non-critical mix ratio: 100 to 40 by weight and 100 to 50 by volume
  • Lower exotherm system; longer working life
  • Outstanding temperature and chemical resistance
  • Reliable electrical insulator
  • Gun dispensable
  • Cryogenically serviceable
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.