Supreme 11HTND

Toughened, two component epoxy for bonding, sealing and coating with paste consistency
Key Features
  • Convenient handling
  • Excellent toughness
  • Withstands thermal cycling
  • High bond strength in shear and peel modes
Typical Properties
Viscosity
Part A: paste, Part B: paste
Cure Schedule
overnight at 75°F, followed by 1 hour at 150-200°F
Hardness
75-85 Shore D
Service Temperature Range
-112°F to +400°F
Tensile Lap Shear Strength
3200-3400 psi
Tensile Modulus
300000-350000 psi
תמונה
Supreme 11HTND Two Component Epoxy System
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond Supreme 11HTND is a high performance, two part epoxy for bonding, sealing and coating with a paste consistency. It is easy to use with a one to one mix ratio by weight or volume. Supreme 11HTND is a faster setting system and cures readily at room temperature or more quickly at elevated temperatures. The optimum curing schedule is overnight at room temperature, followed by 1 hour at 150-200°F. It is formulated to have very good toughness, which imparts high bond strengths in both the shear and peel modes. It also allows the system to withstand rigorous thermal cycling as well as impact and shock. Supreme 11HTND bonds well to a wide variety of substrates, including metals, glass, ceramics, composites, many rubbers and plastics. It has fine chemical resistance to water, oil and fuels. Upon curing, it is a highly reliable electrical insulator. Most noteworthy is its very wide temperature range of -112°F to +400°F. Additionally, Supreme 11HTND has low shrinkage upon curing, dependable dimensional stability and is readily machinable. The color of Part A is gray and Part B is amber. The user friendly processing and top notch performance profile enables Supreme 11HTND to be used in a wide variety of high-tech applications, especially in aerospace, electronics, specialty OEM and related industries.

Product Advantages

  • Convenient handling; 1:1 mix ratio
  • Easy to apply, paste consistency
  • Resists thermal cycling and shock
  • Exceptionally strong in shear and peel modes
  • Good dimensional stability
  • Low shrinkage upon curing
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.