Electrically Insulative, Toughened Epoxy Meets NASA Low Outgassing Specifications
Master Bond Supreme 42HT-2ND Black is a two-part, non-drip epoxy system designed for bonding, sealing and coating applications. It is capable of withstanding temperatures up to 450°F (232°C), and provides a glass transition temperature (Tg) of 130-135°C. The material meets NASA low outgassing standards and is recommended for applications that require vacuum compatibility.
Supreme 42HT-2ND Black is electrically insulative with a volume resistivity greater than 1014 ohm-cm. This compound has a Shore D Hardness of 75-85 at 75°F and withstands rigorous thermal cycling. It passed damp heat reliability testing for 1,000 hours at 85°C and 85% relative humidity. It offers a high strength profile, with a tensile strength of 9,000-10,000 psi and a tensile modulus of 300,000-350,000 psi at 75°F.
With a forgiving mix ratio of 100 to 40 by weight or 100 to 50 by volume, this paste consistency material can be easily applied with the use of a gun dispenser or spatula. It cures at ambient temperature in 2-3 days, or faster with the addition of heat. Adding heat not only speeds up the curing process but also optimizes the overall performance properties. Supreme 42HT-2ND Black is available in standard packaging, double barrel cartridges for gun kits, as well as pre-mixed and frozen syringes.
For Editorial Use
Click below to download this release in the format of your choice.
| צְרוּפָה | גודל |
|---|---|
| Supreme-42HT-2ND-Black_nr.doc (32.5 KB) | 32.5 KB |
| צְרוּפָה | גודל |
|---|---|
| Supreme-42HT-2ND-Black_nr.txt (6.13 KB) | 6.13 KB |
| צְרוּפָה | גודל |
|---|---|
| Supreme-42HT-2ND-Black_nr.html (4.01 KB) | 4.01 KB |
News Release Images
Click an image to download a high resolution version in JPEG format.