MasterSil 711Med

One part medical grade silicone adhesive, sealant for bonding and sealing
Key Features
  • Ultra fast and non-corrosive cure
  • Outstanding electrical insulation properties
  • Bonds well to a wide variety of substrates
  • Conveniently packaged in 30 cc syringes
  • Good sterilization resistance
  • Meets ISO 10993-5 certification
Typical Properties
Viscosity
60,000-80,000 cps
Cure Schedule
Tack-free time, 75°F, >50% humidity 2-5 minutes
Hardness
25-35 Shore A
Service Temperature Range
-75°F to +400°F
Dielectric Constant
2.5
Elongation
300-400%
תמונה
MasterSil 711Med Silicone System
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

Packaging
Product Description

MasterSil 711Med is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed-in-place gaskets. This specialty system is most noteworthy for its very fast and completely non-corrosive cure. MasterSil 711Med is flowable and bonds well to a broad range of substrates, including glass, metals and many plastics. The speed of the cure depends on the thickness of the layer and the humidity; the thinner the layer the faster the cure. It is extremely soft with superb flexibility and elasticity and outstanding electrical insulation properties. The system is resistant to many sterilants including EtO, gamma radiation, glutaraldehyde and other liquid steriliants. MasterSil 711Med is translucent. It is serviceable from -75°F to +400°F. One particularly useful product property is its ability to adhere well to silicone substrates, a commonly used material in medical device manufacturing. Moreover, since the system is totally non-corrosive, it is compatible for medical electronic applications. These special product properties enable the system to be a candidate in a number of different medical device manufacturing situations.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.