EP3HT-LO
One part, heat curing, no mix epoxy system
Key Features
- Not premixed and frozen
- Unlimited working life at room temperature
- Moderate viscosity
- Passes NASA low outgassing
Typical Properties
Viscosity
100,000-200,000 cps
Cure Schedule
250°F for 20-30 minutes or 300°F for 5-10 minutes, followed by 1 to 3 hours at 250 to 300°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +400°F
Tensile Lap Shear Strength
1,600-1,800 psi
Volume Resistivity
>10¹⁴ ohm-cm