EP3HTSDA-2Med

One component, medical grade, electrically conductive epoxy featuring exceptionally high thermal conductivity
Key Features
  • Not premixed and frozen
  • Long open time at ambient temperatures
  • Cures rapidly at 250-300°F
  • Meets ISO 10993-5
Typical Properties
Viscosity
>400,000 cps
Cure Schedule
250°F for 20-30 minutes, 300°F for 5-10 minutes
Hardness
75-85 Shore D
Service Temperature Range
-80°F to +450°F
Thermal Conductivity
45-49 BTU•in/(ft²•hr•°F) W/(m•K)]
Volume Resistivity
<0.001 ohm-cm
תמונה
EP3HTSDA-2Med One Part Silver Filled Epoxy
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

Product Description

Master Bond EP3HTSDA-2Med is a fast curing, one part silver filled epoxy with exceptional electrical and thermal conductivity. It is not premixed and frozen and does not require storage in a freezer. Curing occurs only when heated to 250-300°F. Since it will not cure until heated, its working life is unlimited at room temperature. EP3HTSDA-2Med has a smooth consistency and dispenses easily.

It bonds well to a wide variety of substrates including metals, ceramics, plastics, silicon dies, among others. Although it is a filled system, it still has robust physical strength properties including lap shear strength. Its most prominent features are its low volume resistivity and high thermal conductivity. The filler particles used in this epoxy are exceptionally small (average 2-3 microns, largest less than 20), allowing for ultra thin bond lines and its very low thermal resistance 2-3 x 10-6 K•m2/W.

The temperature range is -80°F to +450°F. It has good resistance to liquid sterilants such as glutaraldehyde, as well as EtO, gamma radiation and similar type sterilants. EP3HTSDA-2Med is easy to use, with very high thermal and electrical conductivity, while meeting the medical grade criteria mentioned previously. It should be considered in applications with medical devices, where heat curing at 250-300°F is possible and the product profile outlined here is desirable.

Product Advantages

  • Single component system, no mixing
  • Not premixed and frozen
  • Highly electrically conductive
  • Impressive thermal conductivity
  • Convenient packaging
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.