Typical Properties
Viscosity
paste
Cure Schedule
15-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output of 20 milliwatts/cm2
Hardness
70-80 Shore D
Service Temperature Range
-80°F to +300°F
Dielectric Constant
3.4
Tensile Modulus
300,000-350,000 psi
תמונה
UV15-7TK1ANV-3 One Part UV Curable Adhesive
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond UV15-7TK1ANV-3 is a one component UV curable polymer system with a paste consistency for high performance bonding, sealing and special encapsulation. This system is 100% reactive and does not contain any solvents or diluents. Its most salient features include superior physical strength properties, low shrinkage upon curing and enhanced non-yellowing stability. UV15-7TK1ANV-3 is not oxygen inhibited and cures readily in 15-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output of 20 milliwatts/cm². The rate of cure depends upon the compound’s distance from the light source, the thickness of the section and the intensity of the light source. It should be noted that the system can cure in sections up to 1/8 inch. It contains no solvents or diluents.

UV15-7TK1ANV-3 bonds well to a wide variety of substrates including glass, metals and plastics, including polycarbonates, acrylics and polyester films. UV15-7TK1ANV-3 offers very good chemical resistance to water, fuels, and oils, among others. It exhibits an exceptional combination of properties including outstanding durability, and good electrical insulation properties, along with fine thermal cycling capabilities. UV15-7TK1ANV-3 is translucent and has a service temperature range of -80°F to +300°F.This system can be used in optical, fiber-optic, electronic, laser, microelectronic and semiconductor applications, when a robust UV curable paste consistency system is desirable.

Product Advantages

  • One component system, no mixing needed
  • Paste consistency
  • Not oxygen inhibited/li>
  • Outstanding dimensional stability
  • High bond strength to many substrates
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.