EP112LS

Two part, heat curing epoxy for potting, encapsulation, coating, sealing and impregnation
Key Features
  • Superb electrical properties
  • Very good temperature resistance
  • Outstanding non-yellowing properties
  • Wonderful optical clarity
Typical Properties
Viscosity
50-200 cps
Cure Schedule
1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Post curing at 350°F will further enhance product properties.
Hardness
75-90 Shore D
Service Temperature Range
-60°F to +450°F
Refractive Index
1.55
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
EP112LS Two Part Heat Curing Epoxy
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP112LS is a very low viscosity two component epoxy resin system for potting, encapsulation, sealing, coating and impregnation. The mix ratio is an easy to use 100:80 by weight. EP112LS offers an exceptionally long open time of 2-3 days or longer. It does require oven curing for a number of hours. A typical cure schedule would be 1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F. Post curing at 350°F will further enhance product properties. Some of the more noteworthy attributes of EP112LS are first class electrical insulation properties, ample physical strength values as well as compelling optical clarity. It is important to understand that all epoxies will yellow especially upon exposure to UV light. What distinguishes EP112LS is its low rate of yellowing when compared to other optical grade epoxies. It bonds very well to a wide variety of substrates, including glass fibers and ceramics, along with metals, composites, glass and many rubbers and plastics. It features good resistance to a variety of chemicals, including water, oils, fuels, acids and bases. EP112LS is serviceable over the wide temperature range of -60°F to +450°F.

It is widely used for potting, sealing, coating and encapsulation applications as well as for impregnating especially when non-yellowing is an important consideration. This is a common issue in electronic, aerospace and opto-electronic environments. Another prominent feature is its ability to retain its electrical insulation profile over a wide temperature range. Even though the cure schedule is somewhat long, EP112LS is a “go to” material for epoxy applications where superior nonyellowing properties are needed.

Product Advantages

  • Low viscosity, very long working life at ambient temperatures; very low exotherm
  • Superb physical strength properties. Solid dimensional stability
  • Impressive electrical insulation characteristics
  • Ideal for impregnation applications
  • Excellent optical clarity and non-yellowing properties
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.