EP113

Two component, optically clear, nanosilica filled epoxy for potting, encapsulating, coating and sealing
Key Features
  • Ultra low viscosity and very long open time
  • Exceptionally low shrinkage upon curing
  • Superior dimensional stability
  • High temperature resistance
  • Stellar electrical insulation
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
500-1,000 cps
Cure Schedule
2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +450°F
Dielectric Constant
3.40
Tensile Modulus
500,000-550,000 psi
תמונה
EP113 Two Component Epoxy
Certifications

ASTM D4060-14 for Abrasion Resistance

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Packaging
Product Description

Master Bond EP113 is a two component, nanosilica filled epoxy system for potting, coating and sealing. The addition of the nano particles enhances the dimensional stability and the already exceptionally low shrinkage upon curing. EP113 has a 100 to 80 mix ratio by weight. It has an unusually low viscosity along with an especially long open time of 2-4 days. It should be noted that EP113 requires oven curing. A typical cure schedule is 2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F, although, a number of variations are possible.

EP113 is a top tier electrical insulator. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics and plastics. As a toughened system, it has good resistance to thermal cycling and shock. When the aforementioned properties are combined with its pronounced low viscosity, it is a highly attractive candidate for potting and encapsulating. Some other positive features include its excellent physical strength profile as well as its chemical resistance to water, oils, acids, bases and fuels. The service temperature range is -100°F to +450°F. EP113 is a versatile, specialty type system that can be used in many different aerospace, electronic and OEM applications where this uncommon blend of product properties is desirable.

Product Advantages

  • Low viscosity
  • Extraordinarily long open time
  • Can withstand rigorous thermal cycling
  • Marvelous electrical insulation properties
  • Great optical clarity
  • Tested for abrasion resistance per ASTM D4060-14
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.