EP114

Two component, optically clear, nanosilica filled epoxy for potting, encapsulating, coating and sealing
Key Features
  • Low viscosity and very long open time
  • Exceptionally low shrinkage upon curing
  • Superior dimensional stability
  • High glass transition temperature
Typical Properties
Viscosity
500-1,500 cps
Cure Schedule
2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F
Hardness
85-95 Shore D
Service Temperature Range
-100°F to +550°F
Glass Transition Temperature (Tg)
210-215°C
Tensile Modulus
>1,000,000 psi
תמונה
EP114 Two Component Epoxy
Certifications

ASTM D4060-14 for Abrasion Resistance

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

ASTM E595 Compliant

Product Description

Master Bond EP114 is a two component, nanosilica filled epoxy system for potting, coating and sealing. The addition of the nano particles enhances the dimensional stability and the already exceptionally low shrinkage upon curing. EP114 has a 100 to 80 mix ratio by weight. It has an unusually low viscosity along with a very long open time of 2-4 days. EP114 requires oven curing. A typical cure schedule is 2-3 hours at 250°F followed by 5-8 hours at 300°F with a 2 hour or longer post cure at 350°F, although a number of variations are possible.

EP114 bonds well to a wide variety of substrates including metals, composites, glass, ceramics and plastics. It is a top tier electrical insulator. Its Tg exceeds 200°C and the service temperature range is -100°F to +550°F. It is highly resistant to water, oils, and fuels. EP114 is optically clear and transmits light very well, especially in the range of 350 to 1600 nanometers. While EP114 is ideally suited for small potting and encapsulation applications, it can also be used for sealing and coating. EP114 should be considered in specialty OEM, electronic, and optical applications where this combination of properties is desirable.

Product Advantages

  • Low viscosity
  • Very long open time
  • First rate electrical insulation properties
  • Tested for abrasion resistance per ASTM D4060-14
  • Withstands 1,000 hours 85°C/85% RH
  • NASA low outgassing approved
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.