EP17TF

One component, toughened epoxy system for bonding, sealing and coating
Key Features
  • High temperature resistant
  • Withstands rigorous thermal cycling
  • Well suited for bonding dissimilar substrates
  • Exceptional tensile lap shear strength
Typical Properties
Viscosity
paste
Cure Schedule
5-6 hours at 300°F followed by a post cure of 4-5 hours at 350°F
Hardness
85-95 Shore D
Service Temperature Range
-150°F to +550°F
Elongation
5-10%
Tensile Lap Shear Strength
8,000-9,000 psi
תמונה
EP17TF One Part Epoxy System
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP17TF is a specially formulated one component, epoxy for bonding, sealing, coating and encapsulating. It features good toughness, high temperature resistance, and exceptionally strong bonding strength. It has a paste consistency that is easy to apply. The cure schedule is 5-6 hours at 300°F. To obtain optimum properties, a post cure for 4-5 hours at 350°F is recommended. EP17TF is 100% reactive, contains no solvents or diluents, and has low shrinkage upon curing.

EP17TF bonds well to similar and dissimilar substrates such as metal, ceramics, plastics and composites. Its lap shear strength is particularly noteworthy. It combines a relatively high glass transition temperature (Tg) of 150-155°C, along with some compliance to compensate for thermal mismatches. This enables the epoxy to be used in applications where rigorous thermal cycling is an integral part of the operational requirements.

EP17TF resists an impressive array of chemicals including acids, bases, fuels, oils and many solvents. The service temperature range is -150°F to +550°F. The color of EP17TF is beige, other colors are available. This product is a reliable electrical insulator, even at higher temperatures. EP17TF should be considered in applications involving aerospace, electronics, oil and chemical processing, and specialty OEM industries where temperature resistance, high bond strength and thermal cycling are significant considerations.

Product Advantages

  • Single component system
  • Paste consistency, easy to apply
  • Accommodates thermal cycling
  • Impressive lap shear strength
  • Superior combination of high temperature resistance, especially for a forgiving type epoxy system
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.