EP21DP12

Two component urethane modified epoxy for bonding, sealing and potting
Key Features
  • Excellent toughness
  • Convenient processing
  • Can withstand rigorous thermal cycling
  • Available in several colors
Typical Properties
Viscosity
Part A: 4,000-8,000 cps, Part B: 11,000-15,000 cps
Cure Schedule
overnight at 75°F followed by 2 to 3 hours at 135-150°F
Hardness
40-50 Shore D
Service Temperature Range
-100°F to +250°F
Dielectric Constant
3.8
Dielectric Strength
450 volts/mil
Tensile Modulus
5,000-15,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
EP21DP12 Two Part Urethane Modified Epoxy
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP21DP12 is a two component, urethane modified epoxy for bonding, sealing and potting applications. It has a forgiving 2 to 1 mix ratio by weight along with a conveniently extended working life. This system cures at ambient temperatures or more readily at elevated temperatures. The optimum cure schedule is overnight at room temperature followed by 2 to 3 hours at 135-150°F. It is 100% reactive and does not contain any solvents or diluents. Also, it contains an air release agent which allows for facilitated degassing.

EP21DP12 bonds well to a wide variety of substrates such as metals, glass, ceramics and many types of rubbers and plastics. The urethane component allows the system to withstand temperature cycling as well as thermal and mechanical shocks more readily than typical epoxies. EP21DP12 has good resistance to water, oils and fuels. It is a dependable electrically isolating material. It generates relatively low exotherm in comparison to other systems and is appropriate for potting applications up to 2-2.5 inches thick. The service temperature range is -100°F to +250°F. It is available in red, green, blue, black and white for identification or cosmetic purposes. This epoxy is an interesting option for bonding and potting where a toughened system along with a distinctive color are desirable features.

Product Advantages

  • Convenient 2:1 mix ratio by weight
  • Long open time
  • Withstands thermal cycling and mechanical shock
  • Good abrasion resistance
  • Available in cans or with a gun type dispensing systems
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.