Typical Properties
Viscosity
Part A: 1,500 - 2,500 CPS, Part B: 5 - 50 CPS
Cure Schedule
overnight at 75°F followed by 3-5 hours at 140-175°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +350°F
Dielectric Strength
440 volts/mil
Refractive Index
1.57
תמונה
EP21LSCL-2 Two Part Epoxy
Certifications

Meets EU Directive 2015/863

ASTM E595 Compliant

Product Description

Master Bond EP21LSCL-2 is a two component, low viscosity epoxy resin system featuring superb optical clarity. This system has a forgiving mix ratio of 100 to 20 by weight. The recommended cure schedule is overnight at room temperature followed by 3-5 hours at 140-175°F. It has exceptionally low exotherm and a long working life of 6 to 8 hours for a 100 gram mass. This compound is 100% reactive and does not contain any solvents or diluents.

EP21LSCL-2 bonds well to a wide variety of substrates including metals, glass, composites, ceramics as well as many rubber and plastic materials. It is a superb electrical insulator. This, along with its low exotherm, permits it to be effective in larger potting and encapsulation applications. This system’s most outstanding feature is its non yellowing properties when compared to other optically clear epoxies. Also noteworthy is its high glass transition temperature, physical strength profile, and low shrinkage upon curing. It has good resistance to water, oils, fuels and outdoor elements. The service temperature range is from -60°F to +350°F. EP21LSCL-2 is an attractive option when a non-yellowing epoxy with good physical strength properties and temperature resistance is desirable.

Product Advantages

  • Low viscosity; easy to apply or pour
  • Low shrinkage upon curing
  • Long open time
  • Highly desirable non-yellowing profile
  • Meets NASA low outgassing specifications
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.