EP21LVMed

Low viscosity, two component epoxy compound
Key Features
  • Meets USP Class VI certification
  • Passes ISO 10993-5 for cytotoxicity
  • Outstanding thermal cycling resistance
  • Cures at room temperature or elevated temperatures
  • Excellent chemical resistance
  • Serviceable from -65°F to +250°F
Typical Properties
Viscosity
Part A: 10,000-14,000 cps, Part B: 11,000-15,000 cps
Cure Schedule
overnight at 75°F followed by 1-2 hours at 150-200°F
Hardness
>70 Shore D
Service Temperature Range
-65°F to +250°F
Dielectric Strength
440 volts/mil
Tensile Lap Shear Strength
>2,800 psi
תמונה
EP21LVMed Two Part Epoxy System
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

USP Class VI Medical

Product Description

Master Bond EP21LVMed is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room temperature or more quickly at elevated temperatures. To optimize the system’s properties and to ensure biocompatibility, a highly recommended cure schedule is overnight at room temperature followed by 2-3 hours at 150-200°F. It has a convenient one to one mix ratio by weight. EP21LVMed produces high strength, durable bonds which hold up well to thermal cycling and resist many chemicals including water, acids, bases and most importantly, EtO, radiation and many cold sterilants. It is serviceable over the wide temperature range of -65°F to +250°F. It bonds well to a variety of substrates including metals, glass, ceramics, wood, rubbers and many plastics. Once cured, EP21LVMed is an outstanding electrical insulator. This, combined with its low viscosity, makes this system an excellent encapsulating and potting epoxy. It fully passes USP Class VI testing for biocompatibility and it is widely used for medical applications. EP21LVMed contains no solvents or diluents. The color of Part A is clear, while the color of Part B is amber.

Product Advantages

  • Convenient mixing: one to one mix ratio by weight
  • Easy application: only contact pressure required while curing; adhesive spreads readily
  • High bonding strength to a wide variety of substrates
  • Superior physical strength properties
  • Good electrical insulation properties; ideal for potting and encapsulation
  • Resists EtO and radiation as well as many chemical sterilants
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.