EP21ND

Two component epoxy compound for high performance applications
Key Features
  • Two component system
  • One to one mix ratio
  • Room temperature curing
  • Non-drip paste
  • For bonding, sealing and coating
  • Chemical resistant
Typical Properties
Viscosity
paste
Cure Schedule
48-72 hours at 75°F
Hardness
>70 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Constant
2.92
Tensile Lap Shear Strength
>2,500 psi
תמונה
EP21ND Two Part Epoxy
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP21ND is a two component, room temperature curing epoxy compound featuring outstanding physical properties, easy processing and a non-drip, pastelike consistency. This system has a non-critical one to one mix ratio by weight or volume. EP21ND has the unusual characteristic of being able to adjust the properties of the cured system by altering the mix ratio. Adding more of Part A (e.g. 2:1 mix ratio) will give a more rigid cure, while adding more of Part B (e.g. 1:2 mix ratio) gives a more forgiving cure. EP21ND produces high strength, durable bonds which hold up well to thermal cycling and resist many chemicals including water, oils, fuels, acids, bases and salts. It bonds well to a variety of substrates including metals, composites, glass, ceramics and many types of rubbers and plastics. Once cured, EP21ND is an excellent electrical insulator. It is serviceable over the wide temperature range of -60°F to +250°F. The color of Part A is gray and Part B is amber, although, a wide variety of additional color choices are also available. This exceptionally versatile system is widely used in the electronic, electrical, computer, appliance, chemical, aerospace and OEM industries.

Product Advantages

  • Convenient mixing: non-critical one to one mix ratio by weight or volume
  • Variable mix ratio feature allows adjusting the type of cure (mentioned above)
  • Easily applied; adhesive spreads smoothly; non-drip application feature
  • Ambient temperature cures or fast elevated temperature cures as required
  • High bonding strength to a wide variety of substrates
  • Excellent dimensional stability with good electrical insulation properties
  • Lower shrinkage upon cure.
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.