Typical Properties
Viscosity
paste
Cure Schedule
48-72 hours at 75°F
Hardness
>70 Shore D
Service Temperature Range
-60°F to +250°F
Tensile Lap Shear Strength
>2500 psi
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
EP21NDFG Two Component Epoxy
Certifications

FDA Food Grade 21 CFR 175.105

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP21NDFG is a two component, room temperature curing epoxy adhesive/sealant featuring outstanding physical properties, easy processing and a non-drip, paste-like consistency. This system has a non-critical one to one mix ratio by weight or volume. EP21NDFG has the unusual characteristic of being able to adjust the properties of the cured system by altering the mix ratio. Adding more of Part A (e.g. 2:1 mix ratio) will give a more rigid cure, while adding more of Part B (e.g. 1:2 mix ratio) gives a more forgiving cure. EP21NDFG produces high strength, durable bonds which hold up well to thermal cycling and resist many chemicals including water, oils, fuels, acids, bases and salts. It bonds well to a variety of substrates including metals, composites, glass, ceramics and many types of rubbers and plastics. Once cured, EP21NDFG is an excellent electrical insulator. It is serviceable over the wide temperature range of -60°F to +250°F. The color of both Parts A and Part B is amber, although, a wide variety of additional color choices are also available. EP21NDFG is primarily used in food equipment applications where there is an indirect exposure to food and related products.

Product Advantages

  • Convenient mixing: non-critical one to one mix ratio by weight or volume
  • Variable mix ratio feature allows adjusting the type of cure (mentioned above)
  • Easily applied; adhesive spreads smoothly; non-drip application feature
  • Ambient temperature cures or fast elevated temperature cures as required
  • High bonding strength to a wide variety of substrates
  • Lower shrinkage upon cure
  • Excellent dimensional stability with good electrical insulation properties
  • Meets FDA Section 175.105 for indirect food applications

Frequently Asked Questions

Which food grade specifications does EP21NDFG meet?

EP21NDFG complies with the FDA 175.105 for indirect food applications.

Is EP21NDFG rated for direct contact with food?

Although EP21NDFG is not rated or qualified for applications involving direct food contact, it is suitable for sustained use in food equipment applications with indirect food contact.

Can EP21NDFG be used to repair items and equipment in a home kitchen?

No. EP21NDFG is only intended for industrial bonding and sealing applications and is not suitable for home use. In order to achieve optimum properties, this epoxy requires post curing (150-200°F) for at least 2 hours, and we highly recommend the use of industrial ovens for the curing process.

Is EP21NDFG rated for contact with potable water?

No. EP21NDFG is not rated or qualified for use in potable water applications.

Although EP21NDFG has passed FDA standards, how important is it for the end user to perform further testing on the final device?

It is the end user’s responsibility to consult with the appropriate agencies as well as their own legal and technical experts, in order to qualify the EP21NDFG in the context of their application, and obtain the necessary approvals for the final device.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.