EP21TP-2NV

Two component, epoxy polysulfide for bonding, sealing, coating and encapsulation
Key Features
  • One to one mix ratio
  • Tough, flexible bonds
  • Withstands thermal cycling
  • Room temperature curing
  • Chemical resistance to fuels, oils, hydrocarbons and hydraulic fluids
  • Fully complies with RoHS regulations


Note: EP21TP-2NV complies with RoHS3 Directive (EU) 2015/863. It is a new version of EP21TP-2, which has been discontinued.

Typical Properties
Viscosity
Part A: 4,500-7,500 cps, Part B: 500-3,000 cps
Cure Schedule
75°F 48-72 hours
Hardness
40-50 Shore D
Service Temperature Range
-80°F to +250°F
Dielectric Constant
3.7
Elongation
40-80%
תמונה
Product Description

Master Bond EP21TP-2NV is a two component epoxy polysulfide system formulated to cure at room temperature or more rapidly at elevated temperatures, with a one to one mix ratio by weight or volume. It’s a versatile material that can be used as an adhesive, coating, encapsulant and especially as a sealant. It resists a wide array of chemicals including water, gasoline, fuels, oils, hydrocarbons, hydraulic fluids and many acids and bases. Significantly, unlike many chemical resistant epoxy based materials, this system has excellent toughness. These properties enable EP21TP-2NV to withstand rigorous thermal cycling as well as mechanical and thermal shocks.

glass, ceramics and many rubber and plastic materials. The cured system has excellent electrical insulation properties. Its service temperature range is -80°F to +250°F. One unusual feature of EP21TP-2NV is the influence of adding heat to the curing cycle. When cured at room temperature the Shore D hardness is 60-65; when cured at 200°F for 2-3 hours, its hardness is 15-20 Shore D. Therefore, to obtain the optimum properties, EP21TP-2NV should be cured at room temperature. The color of Part A is tan and Part B is amber, although, other colors are available. Polysulfide based systems, including EP21TP-2NV, have been used as fuel tank sealants and as potting compounds for electrical connectors exposed to fuels, oils and lubricants, for many years now. EP21TP-2NV is an excellent choice for use as a sealant, adhesive or potting system for aerospace, electronic, electrical, and specialty OEM where room temperature curing, toughness and chemical resistance to fuels and related compounds are desirable.

Product Advantages

  • Convenient mixing: forgiving one to one mix ratio by weight or volume
  • Ambient temperature curing imparts optimal chemical resistance and hardness
  • Produces tough, bonds; resistant to thermal cycling
  • Good hardness and elongation
  • Superior electrical insulator
  • Superb resistance to fuels and related chemicals
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.