EP29LPTCHT

Two component, thermally conductive, electrically insulative epoxy system
Key Features
  • Low exotherm, long working life
  • Applicable in very thin bond lines
  • Excellent flow properties
  • Superior dimensional stability
Typical Properties
Viscosity
5,000-15,000 cps
Cure Schedule
overnight at 75°F followed by 4-5 hours at 160°-180°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +350°F
Coefficient of Thermal Expansion
22-24 x 10⁻⁶ in/in/°C
Dielectric Constant
4.4
תמונה
Two Part Epoxy EP29LPTCHT
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Product Description

Master Bond EP29LPTCHT is a two component epoxy system featuring good thermal conductivity along with being electrically isolating. It has convenient handling with a forgiving 100 to 50 mix ratio by weight. It is a lower viscosity material with excellent flow properties. It generates very little heat even when mixing larger masses. Not surprisingly, it has a very long open time as indicated below. The recommended cure schedule is overnight at room temperature followed by 4-5 hours at 160°-180°F. Also noteworthy is its very low shrinkage upon curing and dimensional stability.

Especially important is the very fine particle size of the thermally conductive filler. When used as an adhesive, this allows bond line thicknesses ranging from 5 to 15 microns, if desired. This translates into significantly lower thermal resistance ranging from 12-15 x 10-6 K•m2/W. Another plus is its low exotherm and good flow. Therefore the epoxy is a viable candidate for large potting and encapsulation.

This epoxy bonds well to a wide variety of substrates including metals, glass, ceramics and many different plastics. EP29LPTCHT is a very good heat conductor while retaining reliable electrical insulation values. It is resistant to water, fuels and oils. Part A is off white and Part B is white. The service temperature range is -60°F to +350°F. To summarize, EP29LPTCHT is best utilized in specialty bonding applications where a low viscosity, longer working life epoxy has exceptionally low thermal resistance.

Product Advantages

  • Lower viscosity and excellent flow properties
  • Long working life at ambient temperatures
  • Exceptionally low thermal resistance
  • Good electrical insulator
  • Ideal for underfill applications
  • Meets NASA low outgassing
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.