EP30-2LB
Two component, room temperature curing, optically clear epoxy for bonding, sealing, coating and encapsulation. Formulated to have special optical properties
Key Features
- Transmits well from 450-900 nm and above
- Blocks UV light (200-400 nm)
- Good structural adhesive
- Excellent electrical insulator
Typical Properties
Viscosity
Part A: 10,000-16,000 cps, Part B: 10-35 cps
Cure Schedule
24-48 hours at 75°F or 2-3 hours at 150-200°F
Hardness
80-90 Shore D
Service Temperature Range
-80°F to +300°F
Refractive Index
1.55
Volume Resistivity
>10¹⁵ ohm-cm
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863
Packaging
וידאו
Product Spotlight: EP30-2LB
Formulated with unique optical properties, Master Bond EP30-2LB blocks UV light from 200-400 nm and allows the transmission of visible light from 450-900 nm.
Beyond its optical properties, EP30-2LB is a reliable structural adhesive. It is dimension …