EP30LTE

Two component, low viscosity, epoxy for bonding, sealing, coating and encapsulating
Key Features
  • Room temperature curing
  • Low viscosity
  • Low shrinkage upon cure
  • Very low coefficient of expansion
  • Superior dimensional stability
  • Serviceable from -100°F to +250°F
Typical Properties
Viscosity
Part A: 5,000-10,000 cps, Part B: 290-500 cps
Cure Schedule
cure at 75°F for 12-24 hours, followed by a post cure of a few hours at 150-200°F
Hardness
85-90 Shore D
Service Temperature Range
-100°F to +250°F
Coefficient of Thermal Expansion
15-18 x 10⁻⁶ in/in/°C
Dielectric Constant
4.5
תמונה
EP30LTE Two Component Epoxy
Product Description

Master Bond EP30LTE is a specialty epoxy system featuring exceptionally low coefficient of thermal expansion (CTE). Also noteworthy is its superior dimensional stability. It can be used in bonding, coating, sealing and encapsulation applications. This lower viscosity system will cure at room temperature or more quickly at elevated temperatures. To optimize the properties, it is recommended to cure at room temperature for 12-24 hours, followed by a post cure of a few hours at 150-200°F. The CTE is in the range of 15-18 x 10-6 in/in/°C; markedly lower than other systems. Additionally, it has good thermal conductivity and is highly electrically insulative. Its linear shrinkage upon curing is exceptionally low, less than 0.01%.

EP30LTE bonds well to a wide variety of substrates including metals, glass, ceramics and many rubbers and plastics. It is 100% reactive and does not contain any solvents or diluents. This system offers excellent resistance to many chemicals, such as water, fuels and oils, as well as a number of acids and bases. It is serviceable over the wide temperature range of -100°F to +250°F. Part A of this system is off white in color and Part B is clear. Master Bond EP30LTE is especially used in aerospace, optical, electronic, specialty OEM and other applications where an ultra low CTE along with dimensional stability is desirable.

Product Advantages

  • 100% reactive, contains no diluents or solvents
  • Very low shrinkage upon cure
  • Lower viscosity; good flow properties — ideal for small to moderate sized castings
  • Exceptionally low thermal expansion coefficient: about 15-18 x 10-6 in/in/°C
  • Good thermal conductivity while still electrically insulative
  • Superior dimensional stability
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.