EP30LTE-2

Two component, room temperature curing epoxy for bonding, sealing, coating and encapsulating with low coefficient of thermal expansion
Key Features
  • Thermally and electrically insulating
  • Good flow properties
  • Low shrinkage upon cure
  • Superior dimensional stability
Typical Properties
Viscosity
70,000-100,000 cps
Cure Schedule
overnight at 75°F followed by 2-4 hours at 150-200°F
Hardness
85-95 Shore D
Service Temperature Range
4K to +250°F
Acoustical Impedance
6.4 MRayl
Coefficient of Thermal Expansion
10-13 X 10⁻⁶ in/in/°C
תמונה
EP30LTE-2 Two Part Epoxy
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Product Description

Master Bond EP30LTE-2 is a two part epoxy with an extraordinarily low coefficient of thermal expansion (CTE). It has a forgiving 100 to 5 mix ratio by weight and cures readily at room temperature or more quickly at elevated temperatures. To obtain optimum properties, a good cure schedule is overnight at room temperature followed by 2-4 hours at 150-200°F. The CTE is extremely low, 10-13 x 10-6 in/in/°C. Additionally, it is highly dimensionally stable and electrically insulative. Very significantly, this epoxy has low linear and volumetric shrinkage upon curing.

EP30LTE-2 bonds well to a wide variety of substrates including metals, glass, ceramics and many rubbers and plastics. It is 100% reactive and does not contain any solvents or diluents. This system offers excellent resistance to many chemicals, such as water, fuels and oils, as well as a number of acids and bases. It is serviceable over the wide temperature range of 4K to +250°F. Part A of this system is off white in color and Part B is clear. EP30LTE-2 is especially used in aerospace, optical, electronic, specialty OEM and other applications where low shrinkage, an ultra low CTE along with superb dimensional stability are important requirements.

Product Advantages

  • Relatively easy processing
  • 100% reactive
  • Good flow properties
  • Exceptionally high compressive strength
  • Cryogenically serviceable
  • Meets NASA low outgassing specifications
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.