EP33

Two component, room temperature curing epoxy for bonding, sealing and coating
Key Features
  • Suitable for bonding, sealing and coating
  • Easy machinability
  • High dimensional stability
  • Serviceable up to +450°F
  • Meets MIL-STD-883J Section 3.5.2 for thermal stability
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 100,000-150,000 cps, Part B: 1,500-3,000 cps
Cure Schedule
75°F: 48-72 hours; 200°F: 1-2 hours
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Tensile Modulus
400,000-450,000 psi
Volume Resistivity
>10¹² ohm-cm
תמונה
Certifications

MIL-STD-883J for Thermal Stability

ASTM E595 Compliant

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Product Description

Master Bond EP33 is a two part, room temperature curing epoxy system used for bonding, sealing and coating featuring high temperature resistance, good dimensional stability and very good chemical resistance. It is also much easier to machine compared to most other epoxies. It has a 100 to 70 mix ratio by weight and a very convenient one to one ratio by volume. This system cures readily at room temperature or more rapidly at elevated temperatures. To optimize its properties, the recommended cure schedule is overnight at room temperature followed by a post cure at 150-200°F for 2-3 hours. Once cured EP33 has an exceptionally high temperature resistance, serviceable up to +450°F. It resists a range of chemicals including water, oils, fuels and many acids and bases. This moderate viscosity system bonds well to a wide variety of substrates including metal, glass, ceramics and many rubbers and plastics. It is a competent electrical insulator. EP33 is 100% reactive and does not contain any diluents or solvents. The color of Part A is gray, Part B is amber. It is widely used in aerospace, electronic, electrical and specialty OEM type applications.

Product Advantages

  • Convenient mixing: one to one ratio by volume
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly
  • High temperature resistance up to +450°F
  • Excellent dimensional stability
  • Easily machinable
  • Radiation resistant
  • Meets NASA low outgassing specifications
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.