EP34LV

Two component, room temperature curing epoxy for bonding, sealing and coating
Key Features
  • Resists up to +450°F
  • Easily machinable
  • Excellent dimensional stability
  • High bond strength
  • Superb electrical insulation properties
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 120,000-170,000 cps, Part B: 1,500-3,000 cps
Cure Schedule
overnight at 75°F followed by a post cure at 150-200°F for 2-3 hours
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
3.9
Tensile Lap Shear Strength
2,200-2,400 psi
תמונה
EP34LV Two Part Epoxy
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Packaging
Product Description

Master Bond EP34LV is a two part, room temperature curing epoxy system for bonding, sealing and coating featuring high temperature resistance, sterling dimensional stability and peerless electrical insulation properties. It is also much easier to machine compared to most other epoxies. It has a 100 to 70 mix ratio by weight and a very convenient one to one ratio by volume. This system cures readily at room temperature or more rapidly at elevated temperatures. To optimize its properties, the recommended cure schedule is overnight at room temperature followed by a post cure at 150-200°F for 2-3 hours. Upon polymerization EP34LV is serviceable from -60°F to +450°F. It resists a range of chemicals including water, oils, fuels and many acids and bases. This moderate viscosity system bonds well to a wide variety of substrates including metal, composites, glass, ceramics and many rubbers and plastics. As previously mentioned, it is a top notch electrical insulator and has an array of superior physical properties. EP34LV is 100% reactive and does not contain any diluents or solvents. The color of Part A is black, Part B is amber. It is widely used in aerospace, electronic, electrical and specialty OEM type applications.

Product Advantages

  • Convenient mixing: one to one ratio by volume
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly
  • High temperature resistance up to 450°F
  • Noteworthy electrical insulation properties
  • Excellent dimensional stability
  • Easily machinable
  • Superb adhesion to a wide variety of substrates
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.