EP37-3FLFAOND

Two component epoxy compound for bonding, sealing and encapsulation
Key Features
  • Convenient handling
  • High flexibility
  • Paste consistency
  • Thermally conductive and electrically insulative
  • NASA low outgassing approved
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: paste, Part B: paste
Cure Schedule
75°F: 2-3 days; 150-200°F: 2-4 hours
Hardness
35-45 Shore D
Service Temperature Range
4K to +250°F
Dielectric Constant
4.9
Tensile Modulus
30,000-40,000 psi
תמונה
Two Part Epoxy EP37-3FLFAOND
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Product Description

Master Bond EP37-3FLFAOND is a two component system for high performance bonding, sealing and encapsulation that is formulated to cure at room temperature or more rapidly at elevated temperatures. It has a convenient one to one mix ratio by weight or volume. It has an unusual blend of properties including high thermal conductivity, excellent electrical insulation properties, good physical strength and a high degree of flexibility. Once cured, the epoxy exhibits striking resistance to shock, vibration, impact and thermal cycling. It withstands many chemicals including water, oil and various solvents. It is a wonderful adhesive that forms strong, flexible bonds to a wide variety of substrates including metals, composites, ceramics and many rubbers and plastics. EP37-3FLFAOND is a paste and will stay in place when curing. It is cryogenically serviceable over the wide temperature range of 4K to +250°F. Parts A and B are off-white in color. Master Bond EP37-3FLFAOND is widely used in the electronic, electrical, computer, opto-electronic, aerospace and specialty OEM industries where electrical insulation and heat transfer are required. The uniqueness of EP37-3FLFAOND lies in the fact that this thermally conductive system retains a high level of flexibility while having the desirable physical characteristics inherent in epoxies.

Product Advantages

  • Convenient mixing: easy to use, non-critical one to one mix ratio by weight or volume
  • High bond strength to a wide variety of substrates
  • Resists rigorous thermal cycling, mechanical and thermal shocks
  • Good overall physical strength properties and chemical resistance
  • Cryogenically serviceable down to 4K
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.