EP3HTND-2Med Black

One part, heat curing, biocompatible epoxy compound with paste consistency
Key Features
  • One component, no mix system
  • USP Class VI and ISO 10993-5 certified
  • Superior physical strength properties
  • Resists repeated sterilization
Typical Properties
Viscosity
paste
Cure Schedule
250°F for 20-30 minutes, 300°F for 5-10 minutes
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +400°F
Tensile Lap Shear Strength
1,600-1,800 psi
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
One Part Epoxy EP3HTND-2Med-Black
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

USP Class VI Medical

Product Description

Master Bond EP3HTND-2Med Black is a one part system that combines easy processing with excellent physical strength and bonding properties. This epoxy has a paste consistency and is formulated not to flow while curing. It is easy to use as it does not require any mixing. This system cures simply by heating at 250-300°F for a relatively short time as noted in the chart below. It should be emphasized that this is not a premixed and frozen type system. Its working life is unlimited as it will not cure until heated to the required temperature. Also, EP3HTND-2Med Black has low shrinkage upon curing. It fully meets USP Class VI specifications as well as ISO 10993-5 for cytotoxicity.

It bonds well to a wide variety of substrates including glass, metals, ceramics and most plastics and has superb physical strength properties. EP3HTND-2Med Black also offers good electrical insulation properties. The service temperature range is -60°F to +400°F. It is 100% reactive and does not contain any diluents or solvents. EP3HTND-2Med Black possesses superior chemical resistance, particularly to chemical sterilants, as well as to other types of sterilization including EtO, radiation and especially autoclaving. This medical grade epoxy is widely used in the manufacturing and production of both disposable and non-disposable devices where superior physical properties, fast curing and high performance are paramount and heat curing at 250°F is feasible.

Product Advantages

  • One part, no mixing needed
  • Unlimited working life at room temperature
  • Easily applied, paste consistency; will not flow while curing
  • Fast curing at 250-300°F
  • Superb resistance to autoclaving, chemical sterilants, radiation and EtO
  • Excellent adhesion to many substrates and superior physical properties
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.