EP40Med
Two component, room temperature curing epoxy with high elongation
Key Features
- Convenient handling, long open time
- Good bond strength in shear and peel
- Exceptional adhesion to polycarbonates and acrylics
- Complies with USP Class VI and ISO 10993-5
Typical Properties
Viscosity
Part A: 9,000-16,000 cps, Part B: 6,000-8,000 cps
Cure Schedule
overnight at 75°F followed by 2-3 hours at 120°F to 150°F
Hardness
50-60 Shore D
Service Temperature Range
-80°F to +250°F
Dielectric Constant
4.1
Elongation
80-90%